Color Change

Fastly switch product production from one color to another in a short time to increase efficiency and reduce cost.

Black Spots

Compeletely clean up plastic machine's screw, barrel and hot-runner system without any irregular black spots in products.

High-Temp Polymer

Right-Clean can be used at a temperature from 120 ℃ to 400 ℃ which is suitable for all Polymers purging from PP, ABS to PEEK, PPSU.

The Innovative Purging Solution

Shorten purging time and reduce purging cost, at the same time!

Our purging solutions are specialised in plastic processing machines including Injection Molding Machine, Extrusion Machine, Blow Molding Machine, Hot Runner System etc.

We prove fast and cost-effective solutions compared with traditional purging compounds and pure low cost resin purging.

Please feel free to request free samples to see the results

Lower Cost

You can use only 5% right-clean purging powder mixed with normal low-cost resin like PP to more efficiently and effectively purge your machines.

Shorter Time

With Right-Clean, you only need to make the well-blended mixture stay in the machine for 5 minutes and then purge them out. Yes, it is just like that simple.

One for all

You don't need to prepare many purging products to suit your versatile Polymers. Right-Clean is designed for all types of Polymers, no headache at all.

Wide Temperature Range

Right-Clean can be used up to 400℃, which is a perfect solution for high temperature Polymer's purging like PEEK, PPSU, PES etc.

How we work

It’s simple and easy!

01

Blend

Blend 1-5 w.t.% purging powder to any kind of polymers like PP or the next produced resin. The purging powder can withstand high temperature up to 400 Celsius degrees.

02

Soaking

Let the mixed blend fill up the machine barrel, then stop the machine and wait for 5 minutes. The indication of the filling up barrel is bubbled polymer melt coming out of the nozzle.

03

Purging

Purging out all the bubbled polymer melt in the barrel and in normal case that will be done of purging. For injection molding, please use high back pressure to enhance cleaning efficacy of screw feeding section.

04

Results

Put the next produced materials into the hoop and start the production to check the part quality. In some difficult cases, there might need to repeat the soaking and purging procedures one more time.

We know how it works!

If your current purging product doesn’t work as you expected – change the purging product, not your expectations.